Preview

Proceedings of the Kabardino-Balkarian State University

Advanced search

Long-term thermo-oxidative aging of phenolic triazine polymers

https://doi.org/10.1234/2221-7789-2025-1-31-36

EDN: YRCYAQ

Abstract

Long-term thermo-oxidative aging of phenolic triazine polymers in the air in isothermal condi- tions at wide temperature range was researched. Also powder samples of the polymers were researched by TGA-method. Activation energy of the destruction reaction was evaluated. The dependences «conversion – time» in isothermal conditions were built by calculation. The discrepancy between the calculated and experi- mental curves is shown which is explained by scale effect.

About the Authors

Viktor A. Dyakonov
JSC "Composite".
Russian Federation

Candidate of Technical Sciences.



Vitaly S. Anshin
JSC "Composite".
Russian Federation

Engineer of JSC "Composite," without rank.



Grigoiy O. Zelenenko
JSC "Composite".
Russian Federation

Engineer of JSC "Composite," without rank.



Eugene S. Nazarov
JSC "Composite".
Russian Federation

Engineer of JSC "Composite," without rank.



References

1. Anshin V.S. Cyanate Ester Monomers and Oligomers. Overview of the Modern Research State and Perspectives // Polymer Science. Series B. 2022. V. 64, N 3. P. 241–270.

2. Tsotsis T.K. Thermo-oxidative aging of composite materials // Ageing of composite. Cambridge, 2008. P. 130–159.

3. Tsiamis A., Iredale R.J., Backhouse R., Hallett S.R., Hamerton I. Liquid processible, thermally stable, hydrophobic phenolic-triazine resin for advanced composite applications // ACS Applied Polymer Materials. 2019. V. 1, N 6. P. 1458–1487.

4. Reghunadhan Nair C.P. Advances in addition-cure phenolic resins // Progress in Polymer Science. 2004. V. 29, N 5. P. 401-498.

5. Conley R.T. Oxidative degradation of phenol-formaldehyde polycondensation initial degradation re- actions // Journal of Applied Polymer Science. 1965. V. 9, N 3. P. 1117–1126.

6. Korshak V.V., Pavlova S.S., Gribkova P.N., Tsirgiladze M.V., Pankratov V.A., Vinogradova S.V. On the mechanism of thermal and thermal oxidative degradation of polymers containing sim-triazine rings//High molecular weight compounds A, 1980. VOL. 22, NO. 8. S. 1714-1722.

7. Jankovic B. Thermal degradation process of the cured phenolic triazine thermoset resin (Primaset PT-30). Part I. Systematic non-isothermal kinetic analysis // Thermochimica Acta. 2011. V. 519, N 1-2. P. 114–124.

8. Vyazovkin S. Evaluation of activation energy of thermally stimulated solid-state reactions under arbi- trary variation of temperature // Journal of computational chemistry. 1997. V. 18, N 3. P. 393–402.

9. Vyazovkin S. Modification of the integral isoconversional method to account for variation in activa- tion energy // Journal of computational chemistry. 2001. V. 22, N 2. P. 178–183.


Review

For citations:


Dyakonov V.A., Anshin V.S., Zelenenko G.O., Nazarov E.S. Long-term thermo-oxidative aging of phenolic triazine polymers. Proceedings of the Kabardino-Balkarian State University. 2025;15(1):31-36. (In Russ.) https://doi.org/10.1234/2221-7789-2025-1-31-36. EDN: YRCYAQ

Views: 7


Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 License.


ISSN 2221-7789 (Print)
ISSN 0000-0000 (Online)